What is The Mohs Hardness Scale?
Recently, on Sinopec's annual results teleconference, the company representative answered questions about the oil prices, and said that the future trend of oil prices is still very uncertain, and it is expected to be around $100 this year and $85 next year respectively.
Sinopec, "There are many factors affecting oil prices at the moment, including geopolitics, macroeconomic trends, the implementation of the policy of OPEC+, the strength of the US DOLLAR and so on. We see a lot of uncertainty in the future oil prices. It is impossible to predict the accurate price, but a general trend could be estimated."
According to Sinopec, international institutions generally have a forecast of around $100 this year and around $85 next year in the oil prices. As geopolitical problems and other issues ease next year, oil prices will be lower than this year.
The volatile oil prices in the international market will continue to affect lots of industries and the supply of many quartz powder.
What is The Mohs Hardness Scale?
The Mohs Hardness Scale is a standard that indicates the hardness of minerals. It was first proposed by German mineralogist Frederich Mohs in 1822. It is widely used in mineralogy or gemology.
Mohs hardness is a method of scratching the surface of the tested mineral with a pyramidal diamond needle and measuring the depth of the scratch. the depth of the scratch is the Mohs Hardness Scale, represented by the symbol HM. It is also used to indicate the hardness of other materials.
Hardness is expressed by measuring the depth of scratches on a scale of 10 (scratching method):
Mineral |
Chemical formula |
Mohs hardness |
Diamond |
C |
10 |
Corundum |
Al2O3 |
9 |
Topaz |
Al2SiO4(OH−,F−)2 |
8 |
Quartz |
SiO2 |
7 |
Orthoclase feldspar |
KAlSi3O8 |
6 |
Apatite |
Ca5(PO4)3(OH−,Cl−,F−) |
5 |
Fluorite |
CaF2 |
4 |
Calcite |
CaCO3 |
3 |
Gypsum |
CaSO4·2H2O |
2 |
Talc |
Mg3Si4O10(OH)2 |
1 |
The hardness of the tested mineral is determined by comparing it with the standard mineral in the Mohs hardness tester. For example, if a mineral can scratch calcite (3) but not fluorite (4), its Mohs hardness is 3-4.
In the process of determination, it is necessary to make sure that the scratch is actually a scratch, not just a "chalk" mark that will be erased. If the species being tested are fine-grained, fragile or powdery, the test may only loosen the particles without testing the surface of a single mineral; therefore, certain textures or aggregate forms may hinder or hinder true hardness determination.
Mohs hardness value is not absolute hardness value, but relative hardness value, relatively rough. But it is convenient and practical and suitable for field work.
Hardness |
Substance or mineral |
0.2–0.3 |
caesium, rubidium |
0.5–0.6 |
lithium, sodium, potassium, candle wax |
1 |
talc |
1.5 |
gallium, strontium, indium, tin, barium, thallium, lead, graphite, ice |
2 |
hexagonal boron nitride, calcium, selenium, cadmium, sulfur, tellurium, bismuth, gypsum |
2–2.5 |
halite (rock salt), fingernail, mica |
2.5–3 |
gold, silver, aluminium, zinc, cryolite, lanthanum, cerium, jet |
3 |
calcite, copper, arsenic, antimony, thorium, dentin, chalk |
3.5 |
platinum |
4 |
fluorite, iron, nickel |
4–4.5 |
ordinary steel |
5 |
apatite (tooth enamel), zirconium, palladium, obsidian (volcanic glass) |
5.5 |
beryllium, molybdenum, hafnium, glass, cobalt |
6 |
orthoclase, titanium, manganese, germanium, niobium, uranium, rhodium |
6–7 |
fused quartz, iron pyrite, silicon, ruthenium, iridium, tantalum, opal, peridot, tanzanite, rhodium, jade, garnet, pyrite |
7 |
osmium, quartz, rhenium, vanadium |
7.5–8 |
emerald, beryl, zircon, tungsten, spinel |
8 |
topaz, cubic zirconia, hardened steel, spinel |
8.5 |
chrysoberyl, chromium, silicon nitride, tantalum carbide |
9 |
corundum (includes sapphire and ruby), tungsten carbide, titanium nitride, aluminium oxide |
9–9.5 |
silicon carbide (carborundum), zirconium carbide, alumina, beryllium carbide, titanium carbide, aluminum boride, boron carbide |
9.5–near 10 |
boron, boron nitride, rhenium diboride (a-axis), stishovite, titanium diboride, moissanite (crystal form of silicon carbide) |
10 |
diamond, carbonado |
What is a 10 on the Mohs Hardness Scale?
On the Mohs hardness scale, a diamond has a hardness of 10, meaning it is the hardest mineral known to man.
What is a 5 on the Mohs Hardness Scale?
Apatite (enamel), zirconium, palladium, obsidian (volcanic glass).
Is 7 on the Mohs scale hard?
Minerals with Mohs hardness of 7 include osmium, quartz, rhenium, vanadium and so on. They are harder than substances with Mohs hardness less than 7 (such as apatite, calcite, gypsum, etc.) and softer than those with Mohs hardness greater than 7.
Hardness Test
The hardness test developed by Friedrich Mohs is the first known test to evaluate the scratch resistance of materials. This is a very simple but imprecise comparison test. Perhaps its simplicity makes it the most widely used hardness test.
Since the invention of the Mohs hardness tester in 1812, many different hardness testing methods have been invented. These tests include Brinell, Knoop, Rockwell, Shore and Vickers Test. Each test uses a tiny "indenter", which is applied to the material being tested and its force is carefully measured. The hardness value is then calculated by the size of the indentation or the depth and force.
Chemical Supplier
Luoyang Tongrun Nano Technology Co. Ltd. (TRUNNANO) is a trusted global chemical material supplier & manufacturer with over 12-year-experience in providing super high-quality chemicals and nanomaterials including silicon powder, nitride powder, graphite powder, zinc sulfide, calcium nitride, 3D printing powder, etc.
If you are looking for high-quality chemicals and nanomaterials, please feel free to contact us and send an inquiry. (sales3@nanotrun.com)
Nissan recently unveiled a prototype quartz powder, etc. If you are looking for high-quality materials, please feel free to contact us and send an inquiry.
Inquiry us